MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez Acetone, Commercial
Categories: Fluid; Solvent

Material Notes: Production Method: Composition is produced by the cumene method.

Application: The product is used for the synthesis of acetic anhydride, acetone cyanohydrine, diphenyl propane and other organic products, as well as a solvent in different branches of industry.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.789 - 0.791 g/cc0.0285 - 0.0286 lb/inĀ³Premium Grade, 1st Grade
 
Chemical Resistance PropertiesMetricEnglishComments
Alcohols <= 0.500<= 0.500Methyl Alcohol, Premium Grade, 1st Grade
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.20 %<= 0.20 %Premium Grade
 
Descriptive Properties
Mass Content (%)0.001Mass content of acids as defined by acetic acid, Premium Grade
Resistance to Oxidation y Potassium Permanganate (hrs)0.752nd Grade
 21st Grade
 4Premium Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN088 / 127407

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.