Nucleated extrusion grade suitable for cast and blown film. Excellent melt stability and good melt strength, plus faster set-up for increased line speeds. Superior grease resistance, toughness, resistance to abrasion, and does not absorb food odors. Testing conducted on dry as molded specimen at 73°F Information provided by Nylene® Global Polymer Solutions. |