MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toray TORAYPEF™ Polyolefin Foam 15020 AP8M Polyolefin Foam Sheet
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: TORAYPEF™ is long, semi-rigid, sheet-like foam that features closed cells produced via electron beam cross-linking. With its features such as light weight, heat insulation, shock-absorbing properties, moldability and non-absorption, the product is widely used in a variety of fields, including molded interior automotive parts, building insulation, joint filler, pipe covers, and other industrial materials as well as daily necessities, health and sports equipment.

TORAYPEF™ is long sheet-like foam featuring an expansion ratio of 5x to 50x and a 100% closed cell structure which exhibits superior cushioning, shock-absorbing and heat insulation properties, water resistance and superior chemical properties, with a wide range of potential applications.

  • Superior Shock-Absorbance. The product exhibits superior resilience and flexibility as well as excellent absorption of impact energy. It combines comfortable cushioning with firmness due to its closed-cell structure.
  • Superior Heat Insulation. The thermal conductivity, water absorption and water vapor transmission rates are extremely low and the product is well suited as a thermal insulation material.
  • Superior Waterproofing and Buoyancy. With its closed-cell structure, the product does not absorb water and shows excellent resistance to water and moisture and is highly buoyant.
  • Superior Aesthetics. Cross-linking via electron beam ensures that the surface is smooth with fine textured bubbles.
  • Superior Workability. Additional processing steps such as cutting, slicing, molding and adhesion are easily achieved.
  • Superior Chemical Resistance. Compared with other plastic foams, TORAYPEF™ is virtually immune to the effects of chemical agents.
Processing:
  • Cutting and Punching. Cutting is generally performed using a vertical cutter but cutting can also be performed using scissors or a razor. Punching and boring can be performed using a Thomson punching machine.
  • Slicing: The product can be easily sliced using a slicing machine which employs a rotating knife.
  • Thermal Fusion Bonding: The product can be thermal fusion bonded to other PEF objects as well as steel or aluminum plating. Work can be performed simply by using a hot air gun or a Teflon-coated thermal plate.
  • Molding: Both vacuum molding and pressure molding are possible. Moldability varies among different product grades; the drawing ratio of PE grades as determined via a straight assay is approximately 0.5 while the drawing ratio of PP grades varies from approximately 0.6–1.0.
  • Surface Treatment: Various surface treatments such as embossing, flocking and printing can be performed.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0670 g/cc0.00242 lb/in³
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.403 MPa203.5 psiTD
 1.696 MPa246.0 psiMD
Elongation at Break 238 %238 %TD
 244 %244 %MD
Compressive Strength 0.169 MPa24.5 psi25% Compression
Tear Strength 7.70 kN/m43.9 pliMD
 9.20 kN/m52.5 pliTD
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.0 %
@Temperature 1.00 °C,
Time 432000 sec
2.0 %
@Temperature 33.8 °F,
Time 120 hour
Shrinkage, TD 1.4 %
@Temperature 1.00 °C,
Time 432000 sec
1.4 %
@Temperature 33.8 °F,
Time 120 hour
 
Descriptive Properties
Gel Fraction (%)52
Thermoforming Ratio0.58H/D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9269 / 248958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.