MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite EM 7302XLD Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: EM 7302XLD is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirable.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 - 1.25 g/ccASTM D792
Water Absorption 0.90 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage 0.0015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 48.0 MPaASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 11.0 GPaASTM D790
Compressive Strength 166 MPaASTM D695
Izod Impact, Notched 270 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 1e+6 Hz
wet; ASTM 150
Dielectric Strength >= 9.80 kV/mm
@Frequency 60 Hz
ST, dry
Dissipation Factor 0.030
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 282 °CPost Baked; ASTM D658A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC

PSUMIT143 / 193948

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.