Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.33 g/cc | 1.33 g/cc |
Bulk Density | 0.817 g/cc | 0.0295 lb/in³ |
| 0.881 g/cc | 0.0318 lb/in³ |
Density | 1.33 g/cc | 0.0480 lb/in³ |
| 1.40 g/cc | 0.0506 lb/in³ |
Melt Density | 1.20 g/cc @Temperature 285 °C | 0.0434 lb/in³ @Temperature 545 °F |
Particle Size | 2500 µm | 2500 µm |
Viscosity Measurement | 0.78 - 0.82 | 0.78 - 0.82 |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell R | 112 | 112 |
| 114 | 114 |
Tensile Strength at Break | 25.0 MPa | 3630 psi |
| 25.0 MPa | 3630 psi |
Tensile Strength, Yield | 57.0 MPa | 8270 psi |
| 58.0 MPa | 8410 psi |
Elongation at Break | 120 % | 120 % |
| 120 % | 120 % |
Tensile Modulus | 2.40 GPa | 348 ksi |
| 2.40 GPa | 348 ksi |
Flexural Yield Strength | 77.0 MPa | 11200 psi |
| 84.0 MPa | 12200 psi |
Flexural Modulus | 2.30 GPa | 334 ksi |
| 2.50 GPa | 363 ksi |
Izod Impact, Notched | 0.270 J/cm @Temperature -40.0 °C | 0.506 ft-lb/in @Temperature -40.0 °F |
| 0.400 J/cm @Temperature 23.0 °C | 0.749 ft-lb/in @Temperature 73.4 °F |
Izod Impact, Unnotched | NB | NB |
| NB @Temperature -40.0 °C | NB @Temperature -40.0 °F |
Izod Impact, Notched (ISO) | 3.10 kJ/m² @Temperature -40.0 °C | 1.48 ft-lb/in² @Temperature -40.0 °F |
| 4.50 kJ/m² @Temperature 23.0 °C | 2.14 ft-lb/in² @Temperature 73.4 °F |
Puncture Energy | 0.800 J @Thickness 2.50 mm, Temperature -40.0 °C | 0.590 ft-lb @Thickness 0.0984 in, Temperature -40.0 °F |
| 1.00 J @Thickness 3.20 mm, Temperature -40.0 °C | 0.738 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
| 1.60 J @Thickness 2.50 mm, Temperature -40.0 °C | 1.18 ft-lb @Thickness 0.0984 in, Temperature -40.0 °F |
| 2.10 J @Thickness 3.20 mm, Temperature -40.0 °C | 1.55 ft-lb @Thickness 0.126 in, Temperature -40.0 °F |
| 15.0 J @Thickness 2.50 mm, Temperature 23.0 °C | 11.1 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
| 18.0 J @Thickness 3.20 mm, Temperature 23.0 °C | 13.3 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
| 26.0 J @Thickness 2.50 mm, Temperature 23.0 °C | 19.2 ft-lb @Thickness 0.0984 in, Temperature 73.4 °F |
| 31.0 J @Thickness 3.20 mm, Temperature 23.0 °C | 22.9 ft-lb @Thickness 0.126 in, Temperature 73.4 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Heat of Fusion | 56.0 J/g | 24.1 BTU/lb |
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F |
| 1.30 J/g-°C @Temperature 80.0 °C | 0.311 BTU/lb-°F @Temperature 176 °F |
| 1.40 J/g-°C @Temperature 100 °C | 0.335 BTU/lb-°F @Temperature 212 °F |
| 1.90 J/g-°C @Temperature 200 °C | 0.454 BTU/lb-°F @Temperature 392 °F |
| 2.10 J/g-°C @Temperature 280 °C | 0.502 BTU/lb-°F @Temperature 536 °F |
Melting Point | 240 °C | 464 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F |
| 69.0 °C | 156 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F |
| 65.0 °C | 149 °F |
|
Descriptive Properties |
---|
Acetaldehyde | <3ppm |
Color, CIE a* | -2.5 ± 1.5 |
Color, CIE b* | 0.3 ± 1.5 |
Color, CIE L* | 77.5 min |
Fines, wt%, max | 0.05 |
Pellet Shape | Cubical |
**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.