MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Label-Lyte® 95 LBM-301 White Opaque OPP Film for Blow Mold Label Applications  (discontinued **)
Categories: Polymer; Adhesive; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: White, one-side treated polypropylene label designed for blow mold label applications. As the label becomes part of the container, the result is a "direct print" look. This film satisfies the demanding blow mold label film converting and application requirements by means of a high stiffness and a rough blow mold ready adhesive layer, which provides outstanding adhesion. The treated print surface is designed for solvent-based gravure inks and conventional offset lithography.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 96.5 microns3.80 mil
Coating Weight >= 64.6 g/m²>= 40.4 lb/ream520
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.550.55430
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
438
Shrinkage, TD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
438
 
Optical PropertiesMetricEnglishComments
Gloss 50 %50 %treated surface; 442
Transmission, Visible 13 %13 %417
 
Descriptive Properties
Gurley Stiffness, MD, mgf55
Gurley Stiffness, TD, mgf125
Wetting Tension, receding COS theta0.88
Yield, in2/lb10700

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin
Braskem H 603 Blow Molding Polypropylene
Braskem RP 647 Polypropylene
Braskem PH 0952 HOMO Polypropylene Homopolymer
Dow 6D83K Polypropylene Random Copolymer Resin

PEXB490 / 37795

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.