MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Engineered Polymers Dexflex® D-160HF TPO  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Data provided by Solvay Engineered Polymers.

A thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications requiring thermal stability over a broad temperature range, excellent low-temperature properties, and durable paintability. D-160HF is an exceptional processing material.

Uses: Bumper fascias, fender extensions, and other flexible components.

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Key Words: Thermoplastic Olefinic Elastomer; Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Linear Mold Shrinkage 0.014 cm/cm0.014 in/inASTM D955
Melt Flow 20 g/10 min20 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ASTM D2240
Tensile Strength, Ultimate 14.7 MPa2130 psiIV, 2 in/min; ASTM D638
Elongation at Break 150 %150 %ASTM D638
Flexural Modulus 0.530 GPa76.9 ksiI.B., TAN, 0.5 in/min; ASTM D790
Gardner Impact >= 31.0 J>= 22.9 ft-lbASTM D3029G
 >= 36.0 J
@Temperature -30.0 °C
>= 26.6 ft-lb
@Temperature -22.0 °F
ASTM D-3029, G
Tear Strength 82.0 kN/m468 pli2 in/min; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
CTE, linear 117 µm/m-°C
@Temperature 20.0 °C
65.0 µin/in-°F
@Temperature 68.0 °F
Modified; ASTM D696

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLA6 / 67970

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.