MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chase Plastics CP Pryme® N100STL Unfilled Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Nylon 6, Unfilled, Super Tough, Lubricant additive, pellet form.

Information provided by Chase Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  29.0 MPa
@Temperature 22.8 °C
4200 psi
@Temperature 73.0 °F
Conditioned; ASTM D638
 44.8 MPa
@Temperature 22.8 °C
6500 psi
@Temperature 73.0 °F
Dry; ASTM D638
Elongation at Break 80 %80 %Dry; ASTM D638
 150 %150 %Conditioned; ASTM D638
Flexural Yield Strength  27.6 MPa
@Temperature 22.8 °C
4000 psi
@Temperature 73.0 °F
Conditioned; ASTM D790
 61.4 MPa
@Temperature 22.8 °C
8900 psi
@Temperature 73.0 °F
Dry; ASTM D790
Flexural Modulus  0.621 GPa
@Temperature 22.8 °C
90.0 ksi
@Temperature 73.0 °F
Conditioned; ASTM D790
 1.79 GPa
@Temperature 22.8 °C
260 ksi
@Temperature 73.0 °F
Dry; ASTM D790
Izod Impact, Notched  8.54 J/cm
@Temperature 22.8 °C
16.0 ft-lb/in
@Temperature 73.0 °F
Dry; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Conditioned; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FConditioned. Unannealed.; ASTM D648
 135 °C275 °FDry.Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C125 °FConditioned. Unannealed.; ASTM D648
 51.7 °C125 °FDry.Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHA911 / 268562

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.