MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Plansee Molybdenum sheet standard quality
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Pure Element

Material Notes:

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 10.2 g/cc
Vapor Pressure 1.00e-9 bar
@Temperature 1800 °C
 5.00e-7 bar
@Temperature 2200 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 200 - 280HV10; depending on thickness
Tensile Strength 500 - 700 MPadepending on thickness
Tensile Strength, Yield 480 - 620 MPadepending on thickness
Elongation at Break 1.0 - 15 %depending on thickness
Modulus of Elasticity 320 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000560 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.20 µm/m-°C
Specific Heat Capacity 0.254 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 142 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Molybdenum, Mo 100 %Impurity level not reported
 
Descriptive Properties
Electron work function4,39 eV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elmet-Starck F-21-5 Pure Molybdenum, Foil
Plansee Molybdenum foil
Elmet-Starck Pure Molybdenum, Sheet Premium Grade PS-100-2
Overview of materials for Brass
Elmet-Starck Pure Molybdenum, Sheet Standard Grade PS-300-2

NPLAM905h / 185671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.