MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® PeelCote™ Epoxy Preimpregnated Peel Ply
Categories: Polymer; Thermoset; Epoxy

Material Notes: PeelCote™ is an innovative, epoxy preimpregnated peel ply used as a manufacturing aid for improving laminate surface quality and as a preparation for bonding and painting operations.

  • Reduced labor and scrap costs in lay-up operation
  • Provides a tacky surface on composite or metal molds
  • Protects the molded part surface during trim and drill steps
  • Improves part quality when using molds in poor condition
  • Reinforcement fabric is easily removed from cured part
  • Leaves a clean, resin matte finish, ready for bonding / paint
  • PeelCote™ is available in 250°F (121°C) and 350°F(176°C) cure Epoxy systems for autoclave, press, or vacuum bag/oven molding processes
  • Available in standard and custom - slit widths up to 60” (152.4 cm)

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9896 WPP Peel Ply
Henkel Hysol EA 9895 WPP Peel Ply Film
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 4581 Quartz
Park Aerospace Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced

PPARK124 / 89396

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.