MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Krytox™ AUT 2245 PFPE Automotive Performance Lubricant
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: AUT grades are formulated with unique additives to provide flexible options for anticorrosion protection for automotive equipment and heavy transportation parts, such as viscous fan clutch bearings, alternators, and idler bearings. Krytox™ AUT 2245 grease addresses a broad range of applications from O-ring to bearing lubrication over a wide temperature range, where corrosion is a potential issue. It is thickened with PTFE and contains sodium nitrite, a traditional anti-corrosion additive. All grease grades in the AUT series are based on Krytox™ AUT 1045 oil, an ISO 100-grade PFPE oil. Krytox™ AUT 1045 should be considered for any automotive application requiring the use of an oil, from bearings and small plastic gear boxes to NVH solutions.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc
@Temperature 0.000 °C
2.00 g/cc
@Temperature 32.0 °F
Volatiles  <= 0.10 %
@Treatment Temp. 66.0 °C,
Time 79200 sec
<= 0.10 %
@Treatment Temp. 151 °F,
Time 22.0 hour
ASTM D2595
 <= 0.50 %
@Treatment Temp. 121 °C,
Time 79200 sec
<= 0.50 %
@Treatment Temp. 250 °F,
Time 22.0 hour
ASTM D2595
 <= 2.0 %
@Treatment Temp. 204 °C,
Time 79200 sec
<= 2.0 %
@Treatment Temp. 399 °F,
Time 22.0 hour
ASTM D2595
Viscosity Measure  2.5 cSt
@Temperature 200 °C
2.5 cSt
@Temperature 392 °F
base oil
 12.5 cSt
@Temperature 100 °C
12.5 cSt
@Temperature 212 °F
base oil
 100 cSt
@Temperature 40.0 °C
100 cSt
@Temperature 104 °F
base oil
 310 cSt
@Temperature 20.0 °C
310 cSt
@Temperature 68.0 °F
base oil
 
Mechanical PropertiesMetricEnglishComments
Oil Separation 4.0 %
@Treatment Temp. 99.0 °C,
Time 108000 sec
4.0 %
@Treatment Temp. 210 °F,
Time 30.0 hour
wt% loss
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -44.0 °C-47.2 °F
 
Descriptive Properties
AppearanceWhite, Creamy Consistency
Bearing Life (hr)5300+ASTM D3336. 10,000rpm @200°C.
Standard NLGI Grade2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDUPJ826 / 254014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.