MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Lubrizol acquired the Isoplast product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccASTM D792
Linear Mold Shrinkage 0.0010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPaASTM D 638
Tensile Strength, Yield 69.0 MPaASTM D638
Elongation at Break 1.8 %ASTM D638
Elongation at Yield 1.8 %ASTM D638
Tensile Modulus 1.20 GPaASTM D638
Flexural Strength 338 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Izod Impact, Unnotched 267 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Dart Drop, Total Energy 14.0 J
@Temperature -29.0 °C
ASTM D3763
 17.0 J
@Temperature 23.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 166 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °CUnannealed; ASTM D648
Glass Transition Temp, Tg 138 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 260 °C
Mold Temperature 93.0 - 121 °C
Drying Temperature 80.0 - 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Conditioned, 60% Glass Filled

PDW062a / 138103

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.