MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt SILVALOY® 604 VTG Grade 1 (BRAZE™ 604 VTG, SILVALOY® B60TV) Copper Silver Tin Brazing Filler Metal (AWS BVAg-18 Grade 1)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 604 (VTG) Grade 1 is a silver base braze filler metal used in making of low temperature seals in vacuum tube components. This product is often used in brazing of ferrous and non-ferrous alloys in a controlled atmosphere or vacuum furnace applications without the use of flux. Silvaloy 604 (VTG) is recommended for brazing of heat exchanges exposed to salt water in marine environment. Salt water exposure may cause dezincification in braze alloys containing zinc, particularly in joints involving copper-nickel tubing. Silvaloy 604 (VTG) is a low temperature, low vapor pressure braze filler metal formulated to meet the need for a composition free from volatile constituents, particularly essential in the brazing of vacuum tubes. Silvaloy 603 can be used where low volatiles is not a requirement. Silvaloy 604 (VTG) filler metal can be used successfully to braze in hydrogen atmospheres without the use of flux. The tin content of this filler metal improves its wetting characteristics on ferrous base alloys over in comparison to binary silver copper braze filler metals.

Available forms: Wire, strip, engineered preforms, specialty preforms, powder and paste.

Information provided by Lucas-Milhaupt.

Key Words: AMS 4773; Fed QQ-B-654 BAg-18
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 9.58 g/cc
Density 0.346 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000241 ohm-cm7.1% IACS
 
Thermal PropertiesOriginal ValueComments
Melting Point 1115 - 1325 °F
Solidus 1115 °F
Liquidus 1325 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1325 - 1550 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd <= 0.0010 %
Carbon, C <= 0.0050 %
Copper, Cu 28.47 - 31.47 %Remainder
Lead, Pb <= 0.0020 %
Other, each <= 0.0010 %High vapor pressure elements.
Other, total <= 0.010 %high vapor pressure elements (Including zinc, cadmium, and lead)
 <= 0.010 %Impurity elements
Phosphorus, P <= 0.0020 %
Silver, Ag 59 - 61 %
Tin, Sn 9.5 - 10.5 %
Zinc, Zn <= 0.0010 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9842 / 254787

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.