MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RESPOL EBANTIX® E303 EBA
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: EBA REPSOL EBANTIX® E303 is a copolymer suitable for blown film applications with good optical and mechanical properties even at low temperatures. The material has very good sealing properties. The butyl acrylate content is 3%.
Applications: Shrink film; Silage film; Heavy-duty bags
Recommended melt temperature 180°C. Processing characteristics of E303 are similar to LDPE and conventional polyethylene extruders are recommended.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Copolymer, Food Contact Acceptable; Good Optical Properties

Uses: Blow Molding Applications; Film; Heavy-duty Bags; Stretch Wrap

Agency Ratings: EU Food Contact

Processing Method: Blown Film

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183
Butyl Acrylate Content 3.0 %3.0 %
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %
@Thickness 0.127 mm
500 %
@Thickness 0.00500 in
Blown Film; ISO 527-3
Film Elongation at Break, TD 700 %
@Thickness 0.127 mm
700 %
@Thickness 0.00500 in
Blown Film; ISO 527-3
Elmendorf Tear Strength MD 400 g
@Thickness 0.127 mm
400 g
@Thickness 0.00500 in
Blown Film; ISO 6383-2
Elmendorf Tear Strength TD 590 g
@Thickness 0.127 mm
590 g
@Thickness 0.00500 in
Blown Film; ISO 6383-2
Dart Drop Test >= 600 g
@Thickness 0.127 mm
>= 1.32 lb
@Thickness 0.00500 in
Blown Film; ISO 7765-1
Film Tensile Strength at Break, MD 25.0 MPa
@Thickness 0.127 mm
3630 psi
@Thickness 0.00500 in
Blown Film; ISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa
@Thickness 0.127 mm
3630 psi
@Thickness 0.00500 in
Blown Film; ISO 527-3
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D1003
Gloss 70 %70 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °F
Blow-up Ratio (BUR) 2.52.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1303 / 311996

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.