MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
IN-102 Nickel Alloy, UNS N06102
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Typical Applications: Superheater and jet engine parts

Tensile property data for bar.

Key Words: IN102, IN 102
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 345 MPa
@Temperature 870 °C
 720 MPa
@Temperature 760 °C
 1100 MPa
@Temperature 650 °C
 1300 MPa
@Temperature 540 °C
 1410 MPa
@Temperature 21.0 °C
Tensile Strength, Yield 200 MPa
@Temperature 870 °C
 285 MPa
@Temperature 760 °C
 400 MPa
@Temperature 540 °C
 400 MPa
@Temperature 650 °C
 505 MPa
@Temperature 21.0 °C
Elongation at Break 47 %
@Temperature 21.0 °C
 48 %
@Temperature 540 °C
 64 %
@Temperature 650 °C
 110 %
@Temperature 760 °C
 110 %
@Temperature 870 °C
Rupture Strength 7400 psi
@Temperature 816 °C,
Time 3.60e+6 sec
 12000 psi
@Temperature 816 °C,
Time 360000 sec
 52000 psi
@Temperature 649 °C,
Time 3.60e+6 sec
 67000 psi
@Temperature 649 °C,
Time 360000 sec
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.50 %
Boron, B 0.0050 %
Carbon, C 0.060 %
Chromium, Cr 15 %
Iron, Fe 7.0 %
Magnesium, Mg 0.020 %
Molybdenum, Mo 2.9 %
Nickel, Ni 67 %
Niobium, Nb (Columbium, Cb) 2.9 %
Titanium, Ti 0.50 %
Tungsten, W 3.0 %
Zirconium, Zr 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Special Metals Nickel 200
RA-333 Nickel Alloy (UNS N06333)
Rene 100 Nickel Alloy (UNS N13100)
Alloy 19® Thermocouple Alloy

MN999 / 150221

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.