MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Atom Adhesives AA-BOND FDA16 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval.

Appearance: Amber

Cure Type: Heat cure or Room Temperature

Benefits:

  • Medium viscosity
  • Class VI approved
  • Low permeability
  • Good resistance
Mix Ratio by weight: 100:33/Resin:Hardener

Typical Application: Bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cccured
Solids Content 100 %100 %uncured
Volatile Organic Compounds (VOC) Content 0.15 g/l0.15 g/luncured
Water Absorption at Saturation 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
uncured
Viscosity 4700 cP4700 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75
@Temperature 25.0 °C,
Time 86400 sec
75
@Temperature 77.0 °F,
Time 24.0 hour
 86
@Treatment Temp. 65.0 °C,
Time 14400 sec
86
@Treatment Temp. 149 °F,
Time 4.00 hour
Shear Strength  14.5 MPa
@Temperature 25.0 °C,
Time 86400 sec
2100 psi
@Temperature 77.0 °F,
Time 24.0 hour
Lap, Alum to Alum
 22.8 MPa
@Temperature 65.0 °C,
Time 14400 sec
3300 psi
@Temperature 149 °F,
Time 4.00 hour
Lap, Alum to Alum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+14 ohm-cm1.20e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.9 µm/m-°C29.4 µin/in-°F
Maximum Service Temperature, Air 145 °C293 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 97.0 °C207 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Huntsman Araldite XU 3903 Water-Based Adhesive/Coating
Hexcel® HexPly® 954-2A Curing Cyanate Resin
Coastal Enterprises EP-76 Epoxy Bonding Adhesive
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive

PATOM026 / 172341

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.