MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook times

Applications: IBCs, Toys, General purpose custom molding, Agricultural storage tanks, Marine parts

Additives: Processing antioxidants, UV stabilizers

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50; Condition A, From compression molded specimens; ASTM D1693
ESCR 10% Igepal® 140 hour
@Temperature 50.0 °C
F50; Condition A, compression molded specimens; ASTM D1693
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 17.3 MPa
@Thickness 3.17 mm
Type IV specimen, 2" per minute test speed, rotomolded samples; ASTM D638
Flexural Modulus 0.780 GPa1% Strain Value from rotomolded samples; ASTM D790
Impact Test 67.8 J
@Thickness 3.17 mm,
Temperature -40.0 °C
rotomolded; ARM Method
 217 J
@Thickness 6.35 mm,
Temperature -40.0 °C
rotomolded; ARM Method
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 204 - 315 °CVaries with the mold shape and construction. Oven will also affect process time.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVA143 / 55044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.