MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem Green PE STN7006 Blown Film Extrusion Low Density Polyethylene
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Description: STN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination among mechanical, optical and stiffness properties. Besides STN7006 has low gels content which ensure a production of excellent appearance films. This product is identified as PE 114 according to ASTM D-4976-04a standard specification. Additives free. The minimum biobased content of this grade is 95%, determined according to ASTM D6866.

Applications: High clarity films for coextruded food packaging, such as: cheese, meat, sausages, sliced ham, etc. Cast films for table cloth, curtains and laminated tissues. Flexible bottles for solids, liquids or pasties products for hygiene and cleanness.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Elmendorf Tear Strength MD 310 gASTM D1922
Elmendorf Tear Strength TD 250 gASTM D1922
Dart Drop Test 170 gF50; ASTM D1709
Film Tensile Strength at Break, MD 25.0 MPaASTM D882
Film Tensile Strength at Break, TD 20.0 MPaASTM D882
1% Secant Modulus, MD 140 MPa2% Secant; ASTM D1709
1% Secant Modulus, TD 170 MPa2% Secant; ASTM D1709
 
Optical PropertiesOriginal ValueComments
Haze 8.5 %ASTM D1003
Gloss 60 %45°; ASTM D2457
 86 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 185 °CProfile

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Braskem Green PE SEB853/72 Blown Film Extrusion Low Density Polyethylene
Braskem Green PE SEB853 Blown and Cast Film Extrusion Low Density Polyethylene
Braskem Green PE SBF0323HC Blown Film Extrusion Low Density Polyethylene
Braskem Green PE SBF0323/12HC Blown Film Extrusion Low Density Polyethylene

PBRASK2018 / 199900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.