MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).

Appearance: Translucent spherical pellets

Uses: Injection molding parts, Translucent

Available in Europe

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccISO 2781
Maximum Moisture Content 0.0500.050
Melt Flow 20 - 35 g/10 min
@Load 8.70 kg,
Temperature 217 °C
20 - 35 g/10 min
@Load 19.2 lb,
Temperature 423 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ISO 868
Tensile Strength, Ultimate 42.0 MPa6090 psiISO 37
Elongation at Break 510 %510 %ISO 37
Tensile Modulus 0.283 GPa41.0 ksiISO 527
50% Modulus 25.0 MPa
@Strain 50 %
25.0 MPa
@Strain 50 %
ISO 37
100% Modulus 26.0 MPa
@Strain 100 %
3770 psi
@Strain 100 %
ISO 37
300% Modulus 33.0 MPa
@Strain 300 %
4790 psi
@Strain 300 %
ISO 37
Rebound 37 %37 %ISO 4662
Tear Strength 220 kN/m1260 pliwith incision; ISO 34B
 240 kN/m1370 pliwithout incision; ISO 34B
Abrasion 5050mm3; ISO 4649
Compression Set  22 %
@Temperature 22.0 °C,
Time 252000 sec
22 %
@Temperature 71.6 °F,
Time 70.0 hour
ISO 815
 34 %
@Temperature 70.0 °C,
Time 86400 sec
34 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 147 °C297 °FA50; ISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 °C104 °FInjection
Nozzle Temperature 210 - 220 °C410 - 428 °FInjection
Zone 1 205 - 215 °C401 - 419 °FInjection
Zone 2 210 - 220 °C410 - 428 °FInjection
Zone 3 215 - 225 °C419 - 437 °FInjection
Zone 4 215 - 225 °C419 - 437 °FInjection
Drying Temperature 105 °C221 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Dew Point -30.0 °C-22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® T5191 Ether Based Thermoplastic Polyurethane
Lubrizol Estane® R185A Thermoplastic Polyurethane
Lubrizol Estane® L194A Thermoplastic Polyurethane
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane

PNOVEON154 / 55423

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.