MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® R2000/40 Silicone Rubber Base
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: R2000/40 Silicone Rubber Base is an all purpose base.

Special features:

  • Good balance of properties
  • Good compression set
  • Good molding qualities
  • Excellent shelf stability
  • Excellent filler acceptance

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 42ASTM D2240
Tensile Strength 1244 psiASTM D412
Elongation at Break 693 %ASTM D412
Tear Strength 120 pliASTM D624
Compression Set 17 %
@Temperature 177 °C,
Time 79200 sec
Method B; WSTM 1114
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -73.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 171 °C
press cured
 
Descriptive Properties
AppearanceTranslucentWSTM 1297

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9903 / 197502

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.