Hostacom TKC 471N NA NATURAL medium melt flow, 1,650 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity, impact and scratch and mar resistance. It is typically used for molded-in color interior applications. Applications: Automotive Parts, Interior Automotive ApplicationsInformation provided by LyondellBasell. |