MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® Care M40 R PEEK, Medical Device Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment. VESTAKEEP® Care M40 R are semi finished goods based on the high viscosity VESTAKEEP® Care M40 G polymer resin. The semi-crystalline polymer features superior thermal and chemical resistance.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Injection molding
Delivery form: Stock shape (rods and plates)
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion, Fatigue resistance, Oil / fuels
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Special Characteristics: Semi-crystalline
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Delivery form: Rods Ø6-20mm,stan.lengths 3000mm, Rods Ø25-60mm,stan.lengths 2000mm, Rods Ø70-100mm,stan.lengths 1000mm, Discs Ø98,4mm,thickness 12-30mm, Discs Ø99,5mm,thickness 12-30mm, Discs Ø84,5mm,thickness 12-30mm
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Water Absorption 0.500 %0.500 %Sim to ISO 62
Melt Flow 11.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
11.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84.084.0ISO 7619-1
Tensile Strength, Yield 110 MPa16000 psiISO 527
Elongation at Break 40.0 %40.0 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 4.05 GPa587 ksiISO 527
Flexural Strength 175 MPa25400 psiISO 178
Flexural Modulus 4.05 GPa587 ksiISO 178
Izod Impact, Unnotched (ISO) 5.50 kJ/m²2.62 ft-lb/in²ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.80
@Frequency 1.00e+6 Hz
2.80
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75-1/-2
Vicat Softening Point  305 °C
@Load 5.10 kg
581 °F
@Load 11.2 lb
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
635 °F
@Load 2.25 lb
50 K/h; ISO 306
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7846 / 324978

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.