MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.

Main Application : Injection Moulding

Special Features : Combining high hardness with excellent mechanical properties and good hydrolysis and microbial resistance.

Information provided by Merquinsa.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength, Yield 40.00 MPa5802 psiISO 527-2/5A/500
Elongation at Break 400 %400 %ISO 527-2/5A/500
50% Modulus 14.0 MPa
@Strain 50 %
14.0 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 19.00 MPa
@Strain 100 %
2756 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 34.00 MPa
@Strain 300 %
4931 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 190 kN/m1080 pliISO 34-1B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 110 °C230 °FISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 °C104 °F
Nozzle Temperature 210 °C410 °F
Zone 1 205 °C401 °F
Zone 2 210 °C410 °F
Zone 3 215 °C419 °F
Zone 4 215 °C419 °F
Dry Time 3.00 hour
@Temperature 100 °C
3.00 hour
@Temperature 212 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer

PMES81 / 101413

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.