MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akrochem Akrosorb® 9675
Categories: Other Engineering Material

Material Notes: Product Description: Akrosorb 9675 is a 72% active dispersion of SR 500 on calcium silicate (crystalline quartz-free). SR 500 is trimethylol propane trimethacrylate (TMPTMA), a trifunctional peroxide coagent with a proprietary scorch retarder added. Because SR 500 is a liquid normally used in smaller quantities, this non-dusting, free-flowing powder aids weigh-up and batch addition.

Applications: Akrosorb 9765 is a highly efficient peroxide coagent for curing of most elastomeric systems. As little as 2 phr of active material will raise the modulus and hardness as well as improve compression set resistance (essentially increasing cross-link density). Alternately, less peroxide needs to be used to reach an equivalent state-of-cure of a formula using peroxide alone. Higher levels of 9675 will continue to raise hardness and modulus while at the same time plasticizing the rubber. High hardness compounds (70 Shore D) can be made that have excellent processibility and better elastomeric properties (compression set resistance) than filler or plastic reinforced rubber. The scorch-retarded acrylate monomer in 9675 allows peroxide cures that can be transfer or injection molded due to lower viscosity and reasonable scorch times.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/cc
 
Descriptive Properties
Active0.72
Appearancetan powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH546 / 315464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.