MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 6003-45A Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 454510 s delay; ASTM D 2240
Tensile Strength at Break 5.38 MPa780 psiDie C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tensile Strength, Yield 1.52 MPa220 psiDie C 0.125 in (3.2 mm); 20 in/min (500 mm/min); 100%; ASTM D 412
Elongation at Break >= 500 %>= 500 %Die C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tear Strength 24.5 kN/m140 pliDie C; ASTM D 624
Peel Strength 3.51 kN/m20.0 pliPC/PBT; 90 degrees, 20 in/min (500 mm/min); ISO 813
 4.21 kN/m24.0 pliPC/PMMA; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set  16 %
@Temperature 23.0 °C,
Time 79200 sec
16 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 66 %
@Temperature 70.0 °C,
Time 79200 sec
66 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 238 °C380 - 460 °F
Mold Temperature 21.1 - 48.9 °C70.0 - 120 °F
Drying Temperature 76.7 °C
@Time 7200 - 14400 sec
170 °F
@Time 2.00 - 4.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 34.5 - 103 MPa5000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy
RTP Company RTP 1899 A X 83675 Polycarbonate/Acrylic Alloy (PC/PMMA), Thin Wall Grade
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy

PQZWA1003 / 90461

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.