MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® 14120 Water-resistant resin for stereolithography, White  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: DSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to production plastics.

Somos® 14120 offers many properties that mimic traditional engineering plastics including ABS and PBT. This makes the material ideal for many applications in the automotive, medical and consumer electronics markets and include:

  • functional prototypes
  • water resistant applications
  • Appearance models with minimal finishing
  • Durable concept models
  • High humidity environment applications
  • RTV patterns

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in producing fast Rapid Prototyping and Additive Manufacturing solutions utilizing all major 3D printing systems including SLA printing technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc
@Temperature 22.0 °C
0.0397 lb/in³
@Temperature 71.6 °F
Water Absorption 0.24 %0.24 %ASTM D570-98
Viscosity 240 cP
@Temperature 30.0 °C
240 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ASTM D2240
Tensile Strength, Yield 45.7 MPa6630 psiASTM D638M
Elongation at Break 7.9 %7.9 %ASTM D638M
Elongation at Yield 3.5 %3.5 %ASTM D638M
Modulus of Elasticity 2.46 GPa357 ksiASTM D638M
Flexural Strength 68.9 MPa9990 psiASTM D790M
Flexural Modulus 2.25 GPa326 ksiASTM D790M
Poissons Ratio 0.230.23ASTM D638M
Shear Modulus 1.00 GPa145 ksiCalculated
Izod Impact, Notched 23.5 J/cm44.0 ft-lb/inASTM D256A
Graves Tear Strength 123 kN/m702 pliASTM D1004
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150-98
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150-98
 3.9
@Frequency 60.0 Hz
3.9
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 14.6 kV/mm371 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear  67.0 µm/m-°C
@Temperature -40.0 - 0.000 °C
37.2 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-00
 93.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
51.7 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-00
 156 µm/m-°C
@Temperature 50.0 - 100 °C
86.7 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-00
 180 µm/m-°C
@Temperature 100 - 150 °C
100 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 53.0 °C127 °FASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FASTM D648-98c
Glass Transition Temp, Tg 44.0 °C111 °FASTM E1545-00
 
Descriptive Properties
AppearanceOpaque White
Dp (mm)0.159Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)64Exposure that gives 0.254mm thickness
Ec (mJ/cm2)13Critical exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV & Thermal Postcure
DSM Somos® ProtoGen™ 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
DSM Somos® DMX-SL™ 100 Extremely tough/durable SL resin for stereolithography

PDSMT016 / 93536

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.