MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PVC-U Polyvinylchloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuous operating temperature is from -15°C to 60°C. It can also be easily solvent, cemented and welded.

Properties include:

  • High mechanical strength, tensile strength and hardness
  • Good insulation properties for electronics
  • High chemical resistance
  • Self-extinguishing
  • Low water absorption
  • Easy to varnish and glue
  • Low impact strength
  • Limited weather resistance
Applications include:
  • Pumps and valve body
  • Gaskets
  • Bearing cages
  • Pipe lines
  • Hand pump pipes
  • Brush basic body
  • Parts in the dental medicine
  • Seat strips
  • Pipes for the mounting of kerfs
  • Lamp box

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %ISO 62
Water Absorption at Saturation 0.50 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868
Ball Indentation Hardness 120 MPaISO 2039
Tensile Strength at Break 30.0 MPaISO 527
Tensile Strength, Yield 51.0 MPaISO 527
Elongation at Break >= 10 %ISO 527
Elongation at Yield 3.0 %ISO 527
Modulus of Elasticity 3.04 GPaISO 527
Flexural Strength 90.0 MPaISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 3.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VKB; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CISO 11359
Thermal Conductivity 0.140 W/m-K
@Temperature 20.0 °C
ISO 22007-4
Melting Point 80.0 °CDIN EN ISO 3146
Maximum Service Temperature, Air 60.0 °CUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °CISO 75
Vicat Softening Point 75.0 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -15.0 °CUL 746B
Glass Transition Temp, Tg 80.0 °CDIN EN ISO 3146
Flammability, UL94 V-0test results without UL registration; UL 94
Oxygen Index 47 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
Chemical ResistanceDIN 8061
CKW Resistanceno
Colorgrey
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceno
Physiological indifferenceyes, EEC
Resistance Against Hot Waterno
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Extruded
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid
GEHR Plastics PVC type II®

PGEHR001 / 79838

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.