MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® EO 8019 One-Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast EO 8019 provides the following product characteristics:

Cure: Heat cure

Application: Potting and Encapsulating

Loctite Stycast EO 8019 epoxy, is a resilient, non-sag, heat cure glass adhesive. Non-sag properties are at room temperature and to 149ºC in a 1/8 inch bead.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccUncured
Density 9.50 lb/galUncured
Viscosity 325000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 76.0 µm/m-°C
@Temperature <=35.0 °C
Below Tg
 263 µm/m-°C
@Temperature >=35.0 °C
Above Tg
Glass Transition Temp, Tg 35.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 149 °C
Alternate
 2.00 hour
@Temperature 121 °C
Recommended
 10.0 sec
@Wavelength 365 nm
Recommneded UV Cure: Ultraviolet (UV) light @ 200 to 600 mW/cm²
Gel Time 20.0 min
@Temperature 149 °C
 40.0 min
@Temperature 121 °C
Shelf Life 6.00 Month
@Temperature -16.0 °C
from date of manufacture
 
Descriptive Properties
AppearanceBlack
Non-Sag0.125 in.Bead @ 149 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7947 / 255432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.