MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 786 S Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; very good hydrolysis and microbial resistance; high mechanical strength; good low-temperature flexibility; Application; Toys; Technical parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ISO 868
Hardness, Shore D 3333ISO 868
Tensile Strength, Ultimate 38.0 MPa5510 psi200 mm/min; DIN 53504
Tensile Stress at Strain  2.00 MPa
@Strain 10 %
290 psi
@Strain 10 %
200 mm/min; DIN 53504
 5.30 MPa
@Strain 50 %
769 psi
@Strain 50 %
200 mm/min; DIN 53504
 7.20 MPa
@Strain 100 %
1040 psi
@Strain 100 %
200 mm/min; DIN 53504
 13.3 MPa
@Strain 300 %
1930 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 591 %591 %200 mm/min; DIN 53504
Tensile Modulus  0.0200 GPa
@Temperature 60.0 °C
2.90 ksi
@Temperature 140 °F
storage; ISO 672-1,-4
 0.0350 GPa
@Temperature 20.0 °C
5.08 ksi
@Temperature 68.0 °F
storage; ISO 672-1,-4
 0.400 GPa
@Temperature -20.0 °C
58.0 ksi
@Temperature -4.00 °F
storage; ISO 672-1,-4
Rebound 32 %32 %Resilience; ISO 4662
Tear Strength 60.0 kN/m342 pli500 mm/min; ISO 34-1
Abrasion 4040mm³, Method A; ISO 4649
Compression Set  30 %
@Temperature 23.0 °C
30 %
@Temperature 73.4 °F
72 hr; ISO 815
 40 %
@Temperature 70.0 °C
40 %
@Temperature 158 °F
24 hr; ISO 815
 30 %
@Temperature 70.0 °C,
Time 86400 sec
30 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 230 °C410 - 446 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °F
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 India
 Near East/Africa
 South and Central America
FeatureRelease agent
FormPellets
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 786 E Polyurethane
Covestro Desmopan® 385 E Polyurethane
DSM Biomedical Bionate® 75D Thermoplastic Polycarbonate Polyurethane (PCU)
Covestro Desmopan® 3385A Polyurethane
Covestro Desmopan® 481 Polyurethane

PB09768 / 92608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.