C41020D7 is a screen printable silver paste designed as a counter electrode in electrochemical Biosensors. This is used as a counter electrode in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries, in conjunction with working electrodes and reference electrodes. The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a system for printing on alumina. Information provided by Gwent Electronic Materials Ltd. |