MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Super Asia Polyblend HP10AN TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: A? FDA, RoHS, REACH, PAHs approval.
B? Medical grade.
C? Low specific gravity.
D? High tensile strength.
E? Excellent elongation.
F? Odorless and Non- toxic
G? Its scrap can 100% revitalized into reusable materials.

Material Appearance:
Form: Granules
Color: Translucent/Customized.

Applications: Sporting Goods, chest expander… etc.

Processing Method: Injection and Extrusion

Information provided by Super Asia Polyblend Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 - 0.930 g/cc0.0314 - 0.0336 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7.0 - 137.0 - 13ASTM D2240
Tensile Strength 4.41 MPa640 psiASTM D412
 3.486 MPa
@Temperature 63.0 °C,
Time 1.80e+6 sec
505.6 psi
@Temperature 145 °F,
Time 500 hour
Heat Resistance; W-O-M
 4.104 MPa
@Temperature 136 °C,
Time 605000 sec
595.2 psi
@Temperature 277 °F,
Time 168 hour
High Temperature Aging; ASTM D573
Elongation at Break 900 %900 %ASTM D412
 747 %
@Temperature 63.0 °C,
Time 1.80e+6 sec
747 %
@Temperature 145 °F,
Time 500 hour
Heat Resistance; W-O-M
 873 %
@Temperature 136 °C,
Time 605000 sec
873 %
@Temperature 277 °F,
Time 168 hour
High Temperature Aging; ASTM D573
Rebound 83 %83 %Elasticity; CNS K1392
Tear Strength Test 1010[kg/cm2], ASTM D624 Die C
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -60.0 °C-76.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUPER052 / 305717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.