MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection cycles and thin wall parts. This product complies with ASTM standard D1248-IA1.

Applications: Lids, covers and caps for frozen food storage. Housewares. Toys and decorative items. Production of Master Batch for dyeing and concentrate of additives such as slip agent, anti-block, anti-static, etc.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C.

Information provided by Dax Resinas

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 - 0.919 g/ccASTM D1505
Melt Index of Compound 25 - 35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7.00 MPaASTM D638
Tensile Strength, Yield 9.00 MPaASTM D638
Elongation at Break 120 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 °CASTM D3418
Vicat Softening Point 78.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Feed Temperature 170 - 210 °C
Die Cooling Temperature 25.0 - 45.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Braskem F7018 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene
Braskem IP2418 LDPE Injection Molding Polyethylene
Braskem PB 608 LDPE Injection Molding Polyethylene

PDAX080 / 29505

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.