MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Stanyl® TW271B3 (PA46+PTFE)-CF15, Dry, 15% Carbon Fiber, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Moisture Absorption 2.60 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 185 MPaISO 527-1/-2
 76.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 84.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 92.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 108 MPa
@Temperature 120 °C
ISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
 5.0 %
@Temperature 120 °C
ISO 527-1/-2
 5.0 %
@Temperature 160 °C
ISO 527-1/-2
 5.0 %
@Temperature 180 °C
ISO 527-1/-2
 5.0 %
@Temperature 200 °C
ISO 527-1/-2
Tensile Modulus 12500 MPaISO 527-1/-2
 5100 MPa
@Temperature 200 °C
ISO 527-1/-2
 5400 MPa
@Temperature 180 °C
ISO 527-1/-2
 5700 MPa
@Temperature 160 °C
ISO 527-1/-2
 6300 MPa
@Temperature 120 °C
ISO 527-1/-2
Flexural Modulus 11000 MPaISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°CISO 11359-1/-2
Melting Point 295 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °CISO 72-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Stanyl® TW200B6 PA46-CF30, Dry, 30% Carbon Reinforced, Heat Stabilized
Envalior Stanyl® TW200F8 PA46-GF40, Dry, 40% Glass Filled, Heat Stabilized
Envalior Stanyl® TW300 PA46, Dry, Heat Stabilized
Envalior Stanyl® TW240F10 PA46-GF50, Dry, 50% Glass Filled, Heat Stabilized
Envalior Stanyl® TW200F3 PA46-GF15, Dry, 15% Glass Filled, Heat Stabilized

PDSM8248 / 184949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.