MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics TR-20 Block Insulation
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: TR-20 Block is a superior, high-temperature insulation for service to 2000°F (1095°C). According to ASTM testing procedures, TR-20 exhibits extremely high resistance to breakage to 2000°F (1095°C). Long, maintenance-free service and maximum operating efficiency is assured by TR-20’s unique combination of low conductivity and high stability. TR-20 is also very low in sulfur and iron, making it highly resistant to attack from atmospheric conditions and greatly reducing the possibility of product contamination.

These products can be manufactured in special shapes to fit.

Features:

  • Low thermal conductivity
  • Block construction 36" x 12"
  • Good high temperature strength
  • Variety of thicknesses up to 7”
  • Resistant to cryolite vapors

    Applications:

  • Side and end wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells, reheat and pusher furnaces, copper reverberatory furnaces, and oil-fired water tube boilers

    Curved Block

  • Interior and exterior use on bustle pipes, hot air pipes, stacks and other curved or circular equipment
  • customer specifications, saving money on both installation and energy costs.

    Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.4245 g/cc0.01534 lb/in³at ambient temperature; ASTM C303
     0.4806 g/cc
    @Temperature 1090 °C
    0.01736 lb/in³
    @Temperature 2000 °F
    ASTM C303
    Loss On Ignition 9.5 %9.5 %
    Porosity 91 %91 %ASTM C493
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.000814 GPa0.118 ksiat ambient temperature; ASTM C203
     0.00149 GPa
    @Temperature 1090 °C
    0.216 ksi
    @Temperature 2000 °F
    ASTM C203
    Compressive Strength 1.66 MPa240 psiat ambient temperature; ASTM C165
     2.69 MPa
    @Temperature 1090 °C
    390 psi
    @Temperature 2000 °F
    ASTM C165
     
    Thermal PropertiesMetricEnglishComments
    Specific Heat Capacity 1.01 J/g-°C0.241 BTU/lb-°F
    Thermal Conductivity  0.0900 W/m-K
    @Temperature 204 °C
    0.625 BTU-in/hr-ft²-°F
    @Temperature 399 °F
     0.100 W/m-K
    @Temperature 316 °C
    0.694 BTU-in/hr-ft²-°F
    @Temperature 601 °F
     0.110 W/m-K
    @Temperature 426 °C
    0.763 BTU-in/hr-ft²-°F
    @Temperature 799 °F
     0.120 W/m-K
    @Temperature 540 °C
    0.833 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.120 W/m-K
    @Temperature 649 °C
    0.833 BTU-in/hr-ft²-°F
    @Temperature 1200 °F
     0.140 W/m-K
    @Temperature 746 °C
    0.972 BTU-in/hr-ft²-°F
    @Temperature 1370 °F
     0.150 W/m-K
    @Temperature 856 °C
    1.04 BTU-in/hr-ft²-°F
    @Temperature 1570 °F
    Maximum Service Temperature, Air 1090 °C2000 °FContinuous
    Shrinkage 4.0 %
    @Temperature 1090 °C
    4.0 %
    @Temperature 2000 °F
    Linear; ASTM C356
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 3.8 %3.8 %
    Alkalis 1.3 %1.3 %
    CaO 10 %10 %
    Fe2O3 1.4 %1.4 %
    MgO 0.70 %0.70 %
    SiO2 73 %73 %
    TiO2 0.20 %0.20 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM021 / 2341

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.