MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Silpak RU-575 Water Clear Polyurethane Plastic
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Silpak RU-575 is an easy 1A:1B, by volume, system that cures quickly to a water clear, strong, plastic. It develops hardness and can be demolded rather quickly. It has a high heat deflection temperature which is useful in certain prototyping applications. This product has low viscosity and a long pot-life which facilitates easy mixing, excellent detail penetration, and easy degassing through vacuum or pressure casting techniques for bubble-free castings.

Features:

  • Crystal clear
  • Resistance to yellowing with UV exposure
  • Can be machined, drilled, and sanded
  • Long working time
  • Low shrinkage upon cure
  • Reproduces fine detail
  • Tough and hard but not brittle
Applications:
  • Prototypes
  • Lenses
  • Model Windows
  • Clear injection plastic parts
  • Decorative objects
  • Encapsulation

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Viscosity 600 cPInitial Mixed
Linear Mold Shrinkage 0.0018 in/in
Storage Temperature 73.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80
Tensile Strength 6800 psi
Elongation at Break 6.0 %
Modulus of Elasticity 133.96 ksi
Flexural Strength 8478 psi
@Strain 5.0 %
Flexural Modulus 150992 psi
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Thickness 6.35 mm
Demold
Pot Life 15.0 min1-lb mix
Shelf Life 6.00 Month
 
Descriptive Properties
ColorWater Clear
Heat Deflection Temp138°F
Max Exotherm228°F
Mix Ratio100A:90Bby weight
 1A : 1Bby volume
Specific Volume26.1 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILPAK009 / 318646

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.