MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Heraeus Clevios™ PH 500 Conductive Sulfonate Polymer for Antistatic Coatings
Categories: Polymer

Material Notes: Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Clevios™ PH 500 is an antistatic material based on PEDOT:PSS – chemistry for electronics applications. This conductive polymer is a highly conductive, homogenized dispersion of Clevios™ P.

Typical applications include the antistatic coating of PET or Polycarbonate films for antistatic trays and blister tapes, films for dust protection of components in the LCD industry, antistatic coating of glass, high quality antistatic-coated papers, and other ESD and dissipative applications

Application Methods: Dipping, Spraying, Printing (including gravure, slot-die)

Information provided by Heraeus, Conductive Polymers Division.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
 1.00 g/cc0.0361 lb/in³
Solids Content 1.0 - 1.3 %1.0 - 1.3 %As Supplied
pH 1.5 - 2.51.5 - 2.5As Supplied
Viscosity 8.0 - 25 cP8.0 - 25 cPAs Supplied
 8.0 - 25 cP8.0 - 25 cP
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00330 ohm-cm0.00330 ohm-cmDried Coating after DMSO addition
Surface Resistivity per Square 150 ohm150 ohm
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C212 °FAs Supplied
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 93 %93 %
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month
@Temperature 5.00 - 10.0 °C
9.00 Month
@Temperature 41.0 - 50.0 °F
in unopened original container
 
Descriptive Properties
Conductive Filler TypeOrganic
Form SuppliedDark Blue Liquid
Material TypeDispersion
OdorNone
Recommended SubstratesDisplay Glass, PC, PET
Solvent Systemaqueous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Heraeus Clevios™ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ S HT Antistatic/Conductive Polymer Coating for Screen Printing
Heraeus Clevios™ S V3 Antistatic/Conductive Polymer Coating for Screen Printing
Heraeus Clevios™ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings

PHERA999e / 149968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.