MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Matte finish, superior durability

Uses: Extrusion – wire and cable, General application

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
ASTM D2240
Tensile Strength 48.3 MPaASTM D412
Elongation at Break 550 %ASTM D412/D638
100% Modulus 0.00700 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0131 GPa
@Strain 300 %
ASTM D412
Tear Strength 71.0 pliTrouser; ASTM D470
Graves Tear Strength 950 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 83H-18, 1000g; ASTM D3389 B
Compression Set 19 %
@Temperature 23.0 °C,
Time 79200 sec
 68 %
@Temperature 70.0 °C,
Time 79200 sec
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -44.0 °C
 
Processing PropertiesOriginal ValueComments
Zone 1 174 °CExtrusion
Zone 2 179 °CExtrusion
Zone 3 185 °CExtrusion
Zone 4 191 °CExtrusion
Adapter Temperature 191 °CExtrusion
Die Temperature 179 °CZone 2, Extrusion
 185 °CZone 1, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CPT C-Flex® R70-051 Clear Biocompatible TPE
Overview of materials for Nylon 66, Unreinforced
CPT C-Flex® R70-046 Clear Biocompatible TPE
CPT C-Flex® R70-028 Opaque Biocompatible TPE
CPT C-Flex® R70-026 Opaque Biocompatible TPE

PNOVEON045 / 55312

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.