MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Sealants & Adhesives Supreme Silicone Kitchen & Bath Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Supreme Silicone Kitchen & Bath sealant is a premium 100% silicone sealant with outstanding adhesion, strong flexibility, and lifetime mold-free product protection. This durable sealant is 100% waterproof, water-ready in as little as 30 minutes, and offers 50% joint movement capability. Ideal for kitchen and bath sealing projects, this formulation can adhere to most common kitchen and bath surfaces. Supreme Silicone Kitchen & Bath sealant is neutral curing, which means it is low in odor and will not blemish most metal finishes. Backed by a lifetime guarantee.

Features: Meets ASTM C-920 Class 50 specifications. 100% more flexibility than Class 25 sealants. 7X stronger adhesion than GE Silicone 1 sealant. Resists mold with lifetime mold-free product protection. 30-minute water-ready. 100% waterproof. Will not blemish most high-end metal finishes such as chrome, bronze and nickel. Neutral cure with low odor. Permanent flexibility. Shrink-proof & crack-proof. Excellent adhesion to wet and dry surfaces. Freeze/thaw stability. Non-paintable.

Applications: Supreme Silicone Kitchen & Bath sealant is used in a wide variety of applications including showers, tubs, sinks, tile, countertops and fixtures, as well as other kitchen and bath applications.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 35 g/l<= 35 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1919ASTM D2240
Tensile Strength 1.57 MPa228 psiASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure
Tack-Free Time 30.0 min0.500 hour50% RH; ASTM C679
Working Life 6.00 - 12.0 min6.00 - 12.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColoralmondGESUPSILKB ALM
 clearGESUPSILKB CLR, SIL2KB CLR
 whiteGESUPSILKB WHT
Consistency / Sag< 0.1 inchesASTM D2202
Joint Movement Capability±50%ASTM C719.
OdorLight Ammonia
UV & Weathering ResistanceExcellent30 yr study
Water Ready30 minutesAs Supplied.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9941 / 265752

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.