MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Pressure Seal 13644 Butyl
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 13644 is a 60 durometer black colored Butyl elastomer, it is formulated with FDA sanctioned materials. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 615 A13 EA14 F17; 3 AA 615 B13 B33 EA14 F17; 4 AA 615 A13 B13 B33 EA14 F17; 5 AA 615 A13 B13 B33 EA14 F17; 2 BA 615 F17; 3 BA 615 A14 B13 F17; 4 BA 615 A14 F17; 5 BA 615 F17

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
 58
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 60
@Treatment Temp. 70.0 °C,
Time 252000 sec
Heat Aged
 62
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1902 psi
 1928.6 psi
@Treatment Temp. 70.0 °C,
Time 252000 sec
Heat Aged
 2025.6 psi
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 500 %
 460 %
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 480 %
@Treatment Temp. 70.0 °C,
Time 252000 sec
Heat Aged
100% Modulus 169 psi
Tear Strength 131 pliDie C
 167 pliDie B
Compression Set 10.8 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
Solid
 12.6 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
Plied
 31.3 %
@Treatment Temp. 100 °C,
Time 79200 sec
Solid
 46 %
@Treatment Temp. 100 °C,
Time 79200 sec
Plied
 52 %
@Treatment Temp. 100 °C,
Time 252000 sec
Solid
 63.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -54.0 °F
Shrinkage 0.40 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL238 / 318448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.