MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Victrex APTIV™ 1300 Series Black Polyetheretherketone (PEEK) Polymer Film
Categories: Polymer; Film; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: APTIV 1300 film is the black version of unfilled semi-crystalline films made from VICTREX™ PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications offering an alternative option to the APTIV 1000 natural product. APTIV 1300 film has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardant, low toxicity of combustion products and low moisture absorption in a film format. Inherently halogen free and providing ease of processing makes APTIV films a technology enabler for OEMs, our customers and end users.

Information Provided by Victrex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc
@Temperature 23.0 °C
1.30 g/cc
@Temperature 73.4 °F
ISO 1183
Thickness 50.0 microns1.97 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD  >= 150 %
@Thickness 0.0500 mm
>= 150 %
@Thickness 0.00197 in
ISO 527-3
 >= 150 %
@Thickness 0.100 mm
>= 150 %
@Thickness 0.00394 in
ISO 527-3
Film Elongation at Break, TD  >= 150 %
@Thickness 0.0500 mm
>= 150 %
@Thickness 0.00197 in
ISO 527-3
 >= 150 %
@Thickness 0.100 mm
>= 150 %
@Thickness 0.00394 in
ISO 527-3
Tensile Modulus  2.30 GPa
@Thickness 0.100 mm
334 ksi
@Thickness 0.00394 in
TD; ISO 527-3
 2.40 GPa
@Thickness 0.100 mm
348 ksi
@Thickness 0.00394 in
MD; ISO 527-3
 2.50 GPa
@Thickness 0.0500 mm
363 ksi
@Thickness 0.00197 in
MD; ISO 527-3
 2.50 GPa
@Thickness 0.0500 mm
363 ksi
@Thickness 0.00197 in
TD; ISO 527-3
Film Tensile Strength at Break, MD  120 MPa
@Thickness 0.0500 mm
17400 psi
@Thickness 0.00197 in
ISO 527-3
 120 MPa
@Thickness 0.100 mm
17400 psi
@Thickness 0.00394 in
ISO 527-3
Film Tensile Strength at Break, TD  110 MPa
@Thickness 0.0500 mm
16000 psi
@Thickness 0.00197 in
ISO 527-3
 110 MPa
@Thickness 0.100 mm
16000 psi
@Thickness 0.00394 in
ISO 527-3
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm
@Thickness 0.0500 mm,
Temperature 23.0 °C
4.00e+16 ohm-cm
@Thickness 0.00197 in,
Temperature 73.4 °F
100V; ASTM D257
Dielectric Strength 190 kV/mm
@Thickness 0.0500 mm,
Temperature 23.0 °C
4830 kV/in
@Thickness 0.00197 in,
Temperature 73.4 °F
0.25 in electrode; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD <= 2.0 %
@Thickness 0.0500 mm,
Temperature 200 °C
<= 2.0 %
@Thickness 0.00197 in,
Temperature 392 °F
TM-VX-84
Shrinkage, TD <= 2.0 %
@Thickness 0.0500 mm,
Temperature 200 °C
<= 2.0 %
@Thickness 0.00197 in,
Temperature 392 °F
TM-VX-84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICTA84b / 320028

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.