MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASI® MP 5434 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP 5434 is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and bases and most organic solvents. This product gives better water and temperature resistance than standard 5 minute epoxy. It was formulated to a 1:1 mix ratio for use in either MMD equipment or side by side dual cartridges for easy dispensing. A handling cure is normally achieved at room temperature within 30 - 60 minutes with full cure in 24 hours. An elevated temperature cure schedule can be used to reach final properties quickly.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccpart B
 1.13 g/ccpart A
Solids Content 100 %
Viscosity 12000 cP
@Temperature 25.0 °C
hardener
 13500 cP
@Temperature 25.0 °C
mixed
 15000 cP
@Temperature 25.0 °C
resin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85 - 90instantaneous reading
Tensile Strength 2200 psi
Elongation at Break 200 %
Adhesive Bond Strength 780 psiLap Shear Lexan/Lexan
 780 psiLap Shear Lexan/Butyrate
Peel Strength 80.0 - 90.0 pli
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.4
@Frequency 1e+6 Hz
Dielectric Strength 400 V/mil
Dissipation Factor 0.040
@Frequency <=1.00e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 65.6 °C
accelerated
Working Life 3.00 - 5.00 minWork time in standard 6" mix head
Gel Time 20.0 min
 
Descriptive Properties
Color / appearanceclear, part A
 clear/light yellow tint part B
Handling Strength30 to 40 min @ 75°F
Mix Ratio1:2 by volume (Part A resin: Part B hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9098 / 233465

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.