MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® NXT 75 Fluoropolymer Resin Modified PTFE Granular Molding Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® NXT 75 is a chemically modified polytetrafluoroethylene polymer. When properly processed, Teflon® NXT 75 exhibits the superior properties typical of the fluoropolymer resins: nonaging characteristics, chemical inertness, heat resistance, toughness and flexibility, low coefficient of friction, nonstick characteristics, negligible moisture absorption, and weather resistance. In addition, this resin offers weldability, improved resistance to deformation under load, increased resistance to permeation of chemicals, and a higher dielectric breakdown voltage. This resin provides a high degree of weldability for applications where the use of elevated pressure and temperature are limited.

Teflon® NXT 75 is a fine-cut resin designed for general compression molding of blocks and sheets and for use as a base resin for compounds. It can be used for such applications as: seal rings, valve seats, bearing pads, linings, encapsulations, and as a base resin for filled compounds. This resin is particularly useful in applications where welding of parts to other fluoropolymers such as PFA or standard PTFE is required, e.g., fluid-handling systems.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.17 g/cc2.17 g/ccASTM D4894
Apparent Bulk Density 0.440 g/cc0.0159 lb/in³ASTM D4894
Porosity 0.00 - 0.50 %0.00 - 0.50 %Void content; FTIR
Particle Size 33 µm33 µmAverage diameter; ASTM D4894
Deformation 3.2 %3.2 %14 MPa load, 23°C; ASTM D621-A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 31.5 MPa4570 psiASTM D4894
Elongation at Break >= 500 %>= 500 %ASTM D4894
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 208 kV/mm5280 kV/in76.2 µm (3 mil) film; ASTM D149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® NXT 85 Chemically Modified Free-Flow Granular Fluoropolymer Molding Resin
Chemours Teflon® NXT 70 Fluoropolymer Resin Modified PTFE Granular Molding Resin
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin

PDU9259 / 104553

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.