MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® BL 3175A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur BL 3175A is a blocked aliphatic polyisocyanate based on hexamethylene diisocyanate (HDI) and dissolved in aromatic 100.

Properties / Applications: Desmodur BL 3175A blocked polyisocyanate is used with hydroxyl-functional coreactants in the formulation of light-stable one-component baking systems with relatively low curing temperatures. Coatings based on Desmodur BL 3175A blocked polyisocyanate are used for the industrial finishing of appliances, coil coating, and can coating, and in the automotive industry for chip-resistant primer-surfacers and topcoats. The properties of coatings based on Desmodur BL 3175A blocked polyisocyanate can be influenced, as with two-component polyurethane systems, by the degree of crosslinking and the choice of the polyol. The cure time and temperature required are also dependent upon the choice of coreactant. Combining Desmodur BL 3175A with hydroxyl-functional polyesters such as Desmophen 670BA gives coatings with high flexibility and hardness. The cure rate can be varied by catalysis without adverse effects on storage. Crosslinking with polyamines or amides may result in limited storage stability. In coil coating systems, adequate crosslinking may be achieved without catalysis at 465°F peak metal temperature (P.M.T.). With the addition of 1% dibutyl tin dilaurate (DBTDL) based on solid resin, a crosslinking temperature of 435°F P.M.T. is possible. Thermal yellowing may occur at temperatures above 320°F (160°C), depending on the baking time and the polyol used. Testing in Florida indicates that Desmodur BL 3175A polyisocyanate provides excellent weather stability comparable to Desmodur N 3390A BA/SN polyisocyanate. Desmodur BL 3175A may also be used as additive to upgrade the flexibility and adhesion of conventional baking systems. As with any product, use of Desmodur BL 3175A in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Solids Content 73 - 77 %
Viscosity 2000 - 4000 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point 51.0 °CSetaflash
 
Descriptive Properties
AppearanceClear, pale yellow liquid
Color<60Hazen
Content<0.2%Free NCO content
 11.1%NCO content, blocked

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNAPOL® LH 898 Polyester Resin
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 88A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 91A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 84A Polyurethane, MDI Ester

PCOVEST0327 / 202110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.