MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CMW® ELKONITE 4050 tungsten, high silver  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Refractory Metal; Tungsten Alloy

Material Notes: This material has been rebranded as a part of the NAECO® ELKON® product line.

ELKONITE® 4050 is a high silver material that uses a special tungsten powder. It is made by the press-sinter-infiltrate method. It was developed especially for use as a combination current carrying and arcing contact for molded case circuit breakers. Its strong structure improves its arc erosion resistance while maintaining good temperature rise and current interruption characteristics. ELKONITE® 4050 has approximately the same silver content as ELKONITE® 50S, but has higher mechanical properties due to its higher sintered strength. It is used in the higher rated household breakers.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 13.4 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 65
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000280 ohm-cm62 % IACS
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 50 %
Tungsten, W 50 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
CMW® D50F Silver Nickel Alloy
CMW® ELKONIUM 46 Silver Alloy
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Silvaloy® A20 Brazing Alloy

NCMW081 / 15895

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.