MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics THERM-A-GAP™ 575-NS Silicone-Free Soft Acrylic Thermally Conductive Gap Filler Pad
Categories: Ceramic; Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Ceramic Filled Acrylic

Description: THERM-A-GAP™ acrylic gap filler pads are used in silicone sensitive applications.

Features/Benefits: Economical with good thermal conductivity; No silicone outgassing or extractable; RoHS compliant and Inherently tacky on both sides for ease of application (No pressure sensitive adhesive option available/necessary)

Typical Applications: Hard disk drives/storage; Optical electronics; Aerospace/Defense; Desktop computers, laptops, servers; Telecommunications equipment and Consumer electronics.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccASTM D792
Thickness 20.0 - 100 microns0.787 - 3.94 milASTM D374
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 7070ASTM D2240
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.20 W/m-K
@Pressure 0.345 MPa
8.33 BTU-in/hr-ft²-°F
@Pressure 50.0 psi
ASTM D5470
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP™ T174 Highly Conformable, Thermally Conductive Gap Filler
Parker Chomerics CHO-THERM® 1646 Non-Insulating Interface Material
Overview of materials for Epoxy, Thermally Conductive
Advanced Ceramics ACL 1085 (C-795) Alumina
96% Alumina, thick-film, as fired

PCHOME322 / 131032

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.