MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Kristalex™ 3085 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Kristalex™ 3085 hydrocarbon resin is a water clear, highly color stable, nonpolar, low molecular weight thermoplastic polymer. This resin is compatible with a wide variety of oils, waxes, alkyds, plastics, and elastomers, and is soluble in many common organic solvents. It is indicated for use in plastics modification, adhesives, coatings, sealants, and caulks. In EVA-based hot melt adhesives, Kristalex™ 3085 is compatible with EVA grades with up to 30% vinyl acetate and is useful in formulating low-color adhesives with good low temperature properties. In styrenic block copolymer based adhesives, Kristalex™ 3085 preferentially associates with the styrenic endblocks, producing lower melt viscosity while maintaining room-temperature cohesion without affecting tack and adhesion properties.

Application/Uses:

  • Alluminum-pigment preparations
  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Excellent thermal stability
  • Intermediate softening point
  • Made from purified aromatic monomers
  • Water-white initial color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  100 cP
@Temperature 180 °C
100 cP
@Temperature 356 °F
Melt
 1000 cP
@Temperature 140 °C
1000 cP
@Temperature 284 °F
Melt
 10000 cP
@Temperature 120 °C
10000 cP
@Temperature 248 °F
Melt
 100000 cP
@Temperature 100 °C
100000 cP
@Temperature 212 °F
Melt
Molecular Weight 650 g/mol650 g/molMz
 1200 g/mol1200 g/molMw. Mw/Mn ratio = 1.8
 1900 g/mol1900 g/molMn
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 39.0 °C102 °F
Ring & Ball Softening Point 85.0 °C185 °FASTM E 28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point<-40°CDACP
 2°CMMAP
 35°COMS
ColorYID

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5334 / 222528

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.