MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA1810T LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Petrothene GA1810 is a series of pelletized linear low density polyethylene resins selected by customers for applications that require maximum strength and toughness. These products offer excellent additive homogeneity, require no transfer equipment modification, and facilitate clean and safe handling. Typical applications include heavy duty shipping sacks, trash can liners, commercial and industrial packaging, as well as food and consumer packaging. The Petrothene GA1810 series offers enhanced film strength, drawdown, toughness and heat seal strength. In addition, these resins have excellent low temperature resistance for applications such as stretch film and frozen food packaging.

Availability: Asia-Pacific; Europe; North America; South & Central America

Application: Agriculture Film; Bags & Pouches; Can Liners; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Lamination Film; Liner Film; Retail Carryout Bags; Shrink Film

Market: Flexible Packaging; Rigid Packaging

Processing Method: BOPP; Cast Film

Attribute: Blown Film; Sheet and Profile Extrusion

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccBase Resin; ASTM D792
 0.923 g/ccProduct; ASTM D792
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 6750 ppmGA1810T
Slip Level 1000 ppmGA1810T
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 620 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Secant Modulus, MD 0.240 GPa1% Modulus; ASTM D882
Secant Modulus, TD 0.290 GPa1% Modulus; ASTM D882
Elmendorf Tear Strength MD 400 gASTM D1922
Elmendorf Tear Strength TD 650 gASTM D1922
Dart Drop Test 200 gF50; ASTM D1709
Film Tensile Strength at Break, MD 52.0 MPaASTM D882
Film Tensile Strength at Break, TD 45.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 105 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 17.0 %ASTM D1003
Gloss 45.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9711 / 324646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.