MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement of the friction and dry sliding behavior. Applications include bearing bushes, structural components subjected to dynamic loads, and sliding plates. Formerly Centrodal G.

Information provided by CENTROPLAST Engineering Plastics GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %in water at 23°C; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 110 MPavalue at 30 sec.; ISO 2039-1
Tensile Strength, Yield 43.0 MPav = 50 mm/min; ISO 527-2
Elongation at Break 15 %ISO 527-2
Tensile Modulus 2.20 GPaISO 527-2
Flexural Modulus 2.00 GPaISO 178
Charpy Impact Unnotched 5.00 J/cm²ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²ISO 179/1eA
Coefficient of Friction, Dynamic 0.19vs. steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mmin transformer oil; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
ISO 11359
Melting Point 166 °C10K/min; ISO 3146
Maximum Service Temperature, Air 100 °CLong Term
 140 °CShort term
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CISO 75-2
Vicat Softening Point 140 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Compliance
 
Descriptive Properties
Food ComplianceyesBGVV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Avient LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer
Overview of materials for Acetal Copolymer, Unreinforced
Asahi Kasei TENAC™-C CF454 Copolymer Acetal (POM), Medium Viscosity, Carbon Fiber Reinforced
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity

PCENTR01 / 27952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.