MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dowhon DHF-70011F FFKM, Copolymer, Oring, Gasket
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Property: good mold release, for various Oring and gaskets

Information provided by SICHUAN DOWHON NEW MATERIALS CO., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.93 g/cc1.93 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
 67
@Temperature 23.0 °C,
Time 252000 sec
67
@Temperature 73.4 °F,
Time 70.0 hour
FUEL C
 68
@Temperature 150 °C,
Time 252000 sec
68
@Temperature 302 °F,
Time 70.0 hour
OIL 903
 71
@Temperature 250 °C,
Time 252000 sec
71
@Temperature 482 °F,
Time 70.0 hour
Aging
Tensile Strength 15.1 MPa2190 psi
 12.276 MPa
@Temperature 23.0 °C,
Time 252000 sec
1780.5 psi
@Temperature 73.4 °F,
Time 70.0 hour
FUEL C
 14.39 MPa
@Temperature 150 °C,
Time 252000 sec
2087 psi
@Temperature 302 °F,
Time 70.0 hour
OIL 903
 14.7829 MPa
@Temperature 250 °C,
Time 252000 sec
2144.08 psi
@Temperature 482 °F,
Time 70.0 hour
Aging
Elongation at Break 230 %230 %
 222.64 %
@Temperature 250 °C,
Time 252000 sec
222.64 %
@Temperature 482 °F,
Time 70.0 hour
Aging
 238.97 %
@Temperature 23.0 °C,
Time 252000 sec
238.97 %
@Temperature 73.4 °F,
Time 70.0 hour
FUEL C
 245.64 %
@Temperature 150 °C,
Time 252000 sec
245.64 %
@Temperature 302 °F,
Time 70.0 hour
OIL 903
Compression Set 17 %
@Temperature 200 °C,
Time 252000 sec
17 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -17.0 °C1.40 °FTR10
Brittleness Temperature -25.0 °C-13.0 °F
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWHON063 / 315975

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.