MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass/Carbon Fiber, 30/10% Filler by Weight

Features: Flame Retardant

UL File Number: E157318

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³ASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm
@Thickness 3.17 mm
0.015 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength 128 MPa18500 psiASTM D638
Elongation at Yield 2.0 %2.0 %ASTM D638
Flexural Yield Strength 200 MPa29000 psiASTM D790
Flexural Modulus 10.7 GPa1550 ksiASTM D790
Izod Impact, Notched 0.481 J/cm
@Thickness 3.17 mm
0.900 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.8 µm/m-°C11.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 204 °C400 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PBT GF30 FR 30% Glass Filled
Techmer ES HiFill FR® PBT GF30 FR X 30% Glass Filled
Techmer ES HiFill FR® PBT GF30 FR-S 30% Glass Filled
Techmer ES HiFill FR® PBT GF30 FR-S AS 30% Glass Filled
Techmer ES HiFill® PBT GF30 30% Glass Filled

PTPC0726 / 136664

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.